Hi everyone!! I ask for help because I should reproduce a traction test on Patran / Nastran, to verify that the sigma / epsilon curve I entered as Field is actually the one reproduced by the simulator, I would like to verify it through a graph of the final results between stress tensor / deformation . To do this I did:
- made a parallelepiped shaped specimen
- created field
- given the characteristics to the linear elastic and elastoplastic material with the field
-constrained one side of the parallelepiped
-applied pressure to the opposite side so as to keep the specimen in traction
-mesh
- results and graph, but I always get a linear graph, although I have inserted the complete curve up to break.
I did everything with a non-linear SOL400 analysis.
Would you have any suggestions to be able to get the complete curve ??
As you are using sol400, define field with equivalent plastic strain v/s true stress data, use large displacement, large strain formulation. Also use advanced elements PSHLN1, PSLDN1 .. and carry out the nonlinear analysis. Check plastic strain results to make sure material yields under applied load. Then plot the stress strain curve.
You can refer to Chapter 17: Double Sided Contact - in Nastran demonstration manual.
As you are using sol400, define field with equivalent plastic strain v/s true stress data, use large displacement, large strain formulation. Also use advanced elements PSHLN1, PSLDN1 .. and carry out the nonlinear analysis. Check plastic strain results to make sure material yields under applied load. Then plot the stress strain curve.